One night, a fire flashed at the door of the refrigerated warehouse and the cables burned. After a while, the fire went out, but it also burned the cable. This cutoff also cut off the power to the warehouse. The five or six tons of seafood in the warehouse quickly went bad and smelly because they were not kept fresh. The owner of the cargo, Mr. Liu, suffered heavy losses. The warehouse was newly built when the accident occurred, and the cables were also newly purchased. Logically speaking, the quality should not be so poor. Therefore, Mr. Liu took the cable manufacturer to court.
was entrusted by the court and our company accepted the task of identifying and analyzing the cause of the power outage in the refrigerated warehouse involved.
identification and analysis results: The
identification and analysis expert team went to the site for inspection and made a preliminary observation of the burned cable. They found that the strength of the outer insulating adhesive layer at the break was very low and could be torn apart with force. The inner wires also looked thinner and showed signs of melting.
Then, the expert team took samples and sent them to the laboratory for testing. At the same time, they asked the merchant for relevant production technical qualification information, but the merchant failed to provide it.
concluded from laboratory test results that the outer material of this batch of cables did not meet the relevant regulations and the strength was too low. If the diameter of the wire is too small and the current exceeds the endurance range, it will melt at high temperature or even burn on its own.
This batch of cables is of poor quality and does not meet national standards. In fact, the investigation found that the cable manufacturer did not have relevant production qualifications and the product was a three-no product.